An environmentally friendly and energy-saving coal combustion-supporting agent is composed of 10% potassium permanganate, 15% nitric acid, 20% calcium chloride, 14% iron oxide, 29% calcium oxide and 12% aluminum oxide. It is made up of many kinds of oxides, tackifiers, catalysts and sulfur curing agents. Through coke removal and scaling, oxygen expansion, smoke elimination and dust removal, desulfurization and other links, coal combustion can be fully burned, thermal efficiency can be improved, and the emission of dust and acid gas can be reduced. It is suitable for different boilers, such as hand-fired and machine-fired boilers. It is easy to make briquette. It can remove ash deposit on the heating surface of boilers, intensify combustion, loosen coal seam, increase furnace temperature and reduce smoke blackness.
【技術實現步驟摘要】
一種環保、節能煤炭助燃劑
本專利技術涉及一種煤炭添加劑,尤其是環保、節能煤炭助然劑的配方。
技術介紹
現有的工業、民用嫩料煤炭添加劑僅側重助燃效果,單一從供氧角度考慮,有的助姍添加劑采用焦碳粉、木炭等原料增燃,不能起到節約煤炭,減少有害氣體排放的作用。且不能溶于水,使用上很不方便。有的助燃添加劑單一從供氧角度考慮,持續時間短,瞬間作用強,煤炭中的可燃物質不能充分然燒,且煙氣中的有害物質排放超標.還有的添加劑克服了傳統的煤炭助燃劑瞬間釋放氧氣的弊端,燃燒中的煤炭能得到充分的裂解、嫩燒、充分釋放能量,減少有害氣體排放量,但其本身對鍋爐受熱面的除焦脫垢效果不明顯,仍有熱效率的損失。
技術實現思路
本專利技術為克服現有煤炭添加劑的種種不足,提供一種環保、節能煤炭助燃劑,由多種氧化物,翻粘劑,催化劑,硫固化劑等配制而成,經除焦脫垢,增氧膨松,消煙除塵,脫硫等環節使然煤得以充分燃燒,提高熱效率,減少粉塵和酸性氣體的排放。本專利技術為解決其技術問盈所采取的技術方案是由高錳酸鉀10%、硝酸銨15%、氯化鈣2俄、三氧化二鐵14%、氧化鈣29%、三氧化二鋁12%構成。本專利技術的有益效果是,適用于手燒、機燒等不同的鍋爐,便于制作型煤,能清除鍋爐受熱面外表積灰,強化燃燒,疏松煤層,提高爐膛溫度,降低排煙黑度,符合一類地區煙塵排放環保標準。具體實施方式:本專利技術是由高錳酸鉀10%、硝酸錢15%、氧化鈣20%、三氧化二鐵14%、氧化鈣2外、三氧化二鋁1器構成。按配方比例將原料混勻,經檢驗即得產品。由于本配方中的原料均溶于水,可根據需要制備成固體粉狀、液體水劑。使用時,粉狀助燃劑按煤的 ...
【技術保護點】
1.一種環保、節能煤炭助燃劑,其特征是由下列成分組成:高錳酸鉀10%、硝酸銨15%、氧化鈣20%、三氧化二鐵1錢、氧化鈣29%、三氧化二鋁12%。
【技術特征摘要】
1.一種環保、節能煤炭助燃劑,其特征是由下列成分組成:高錳酸鉀10%、硝...